AUTONIC Processes |
|
Autonic Processes are available in seven basic formulations delivering specific deposit properties. Phosphorus contents range from 4.5% to over 13% and operate from a pH of 3.5 to 9.5. Products are provided in a Production Formula that includes Sodium hypophosphite and a Matrix Formula that uses customer supplied Sodium hypophosphite. |
Product Summary |
|
SEM of Autocatalytic Nickel surface showing a 100nm layer of NiO + PO surface passivation layer. |
|
To contact us: |
|
Processes |
|
Matrix |
|
Production |

|
MX |
7-10% P |
Engineering Deposit, Low Stress |
MXMA, MXMC, MXMD Hypophosphite LNS |
MXPA MXPC LNS |
|
MB |
7-10% P |
Bright Deposit, Decorative Applications |
MBMA, MBMC, MBMD Hypophosphite LNS |
MBPA MBPC LNS |
|
LX |
4.5-8% P |
Low Phosphorus, Wear Applications |
LXMA, LXMC, LXMD Hypophosphite LNS |
LXPA LXPC LNS |
|
LB |
4.5-8% P |
Low Phosphorus, Decorative Applications |
LBMA, LBMC, LBMD Hypophosphite LNS |
LBPA LBPC LNS |
|
LE |
4.5-8% P |
Low Phosphorus, IR Absorber |
LEMA, LEMC, LEMD Hypophosphite LNS |
LEPA LEPC LNS |
|
HX |
10-13% P |
High Phosphorus, Corrosion Resistant |
HXMA, HXMC, MXMD Hypophosphite LNS |
HXPA HXPC LNS |
|
HB |
10-13% P |
High Phosphorus, Brightened |
HBMA, HBMC, HBMD Hypophosphite LNS |
HBPA HBPC LNS |